{"product_id":"tungsten-electrode-wl20","title":"WL20 2% Lanthanated TIG Tungsten Electrodes","description":"\u003cp\u003eWL20 (EWLa-2) is a blue-tip 2% lanthanated tungsten for stable starts and broad AC or DC TIG use, including modern inverter machines.\u003c\/p\u003e\n\u003ch3\u003eWhy Choose WL20\u003c\/h3\u003e\n\u003cp\u003eWL20 is the broad-use option in this range. Its 2% lanthanated composition supports reliable starting and a stable arc in both AC and DC TIG applications without the thorium used in WT20 electrodes.\u003c\/p\u003e\n\u003ch3\u003eKey Specifications\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003eClassification:\u003c\/strong\u003e WL20 \/ EWLa-2\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003eComposition:\u003c\/strong\u003e 2% lanthanated tungsten\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003eCurrent:\u003c\/strong\u003e AC or DC\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003eColor code:\u003c\/strong\u003e Blue\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003eLength:\u003c\/strong\u003e 7\" (175 mm)\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003ePackage:\u003c\/strong\u003e 10 electrodes, vacuum sealed\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003eDiameter options:\u003c\/strong\u003e .040\" (1.0 mm), 1\/16\" (1.6 mm), 3\/32\" (2.4 mm), and 1\/8\" (3.2 mm)\u003c\/li\u003e\n\u003c\/ul\u003e","brand":"YesWelder","offers":[{"title":".040\"","offer_id":45530416808045,"sku":"WL20-1.0-AL","price":20.0,"currency_code":"USD","in_stock":true},{"title":"1\/16\"","offer_id":45530416840813,"sku":"WL20-1.6-AL","price":28.0,"currency_code":"USD","in_stock":true},{"title":"3\/32\"","offer_id":45530416873581,"sku":"WL20-2.4-AL","price":65.0,"currency_code":"USD","in_stock":true},{"title":"1\/8\"","offer_id":45530416906349,"sku":"WL20-3.2-AL","price":89.0,"currency_code":"USD","in_stock":false}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0024\/3249\/9821\/files\/WL20-3.2_02250b49-8c35-49df-bbb6-b5a7812b4dc7.jpg?v=1763976410","url":"https:\/\/pay.yeswelder.com\/products\/tungsten-electrode-wl20","provider":"YesWelder","version":"1.0","type":"link"}