{"product_id":"stainless-steel-mig-solid-wire-er308l","title":"ER308L Stainless Steel MIG Wire","description":"\u003cp\u003eER308L is a low-carbon solid MIG wire for 304\/304L and related stainless steels. Its ≤0.03% carbon content supports corrosion-resistant welds in fabrication, tanks, food equipment, and repair work; external shielding gas is required.\u003c\/p\u003e\n \u003ch3\u003eMaterials and Applications\u003c\/h3\u003e\n \u003cul\u003e\n  \u003cli\u003e304 and 304L stainless steel\u003c\/li\u003e\n  \u003cli\u003e308 and 308L stainless steel\u003c\/li\u003e\n  \u003cli\u003e321 and 347 stainless steel\u003c\/li\u003e\n  \u003cli\u003eStainless fabrication, tanks, food equipment, and repair work\u003c\/li\u003e\n \u003c\/ul\u003e\n \u003ch3\u003eKey Specifications\u003c\/h3\u003e\n \u003cul\u003e\n  \u003cli\u003e\n\u003cstrong\u003eClassification:\u003c\/strong\u003e ER308L\u003c\/li\u003e\n  \u003cli\u003e\n\u003cstrong\u003eProcess:\u003c\/strong\u003e MIG\u003c\/li\u003e\n  \u003cli\u003e\n\u003cstrong\u003eCarbon content:\u003c\/strong\u003e ≤0.03%\u003c\/li\u003e\n  \u003cli\u003e\n\u003cstrong\u003eShielding gas:\u003c\/strong\u003e Argon-based MIG shielding gas; follow the applicable welding procedure\u003c\/li\u003e\n  \u003cli\u003e\n\u003cstrong\u003eSpool weight:\u003c\/strong\u003e 2 lb (0.9 kg)\u003c\/li\u003e\n  \u003cli\u003e\n\u003cstrong\u003eSpool diameter:\u003c\/strong\u003e 4\" (102 mm)\u003c\/li\u003e\n  \u003cli\u003e\n\u003cstrong\u003eDiameter options:\u003c\/strong\u003e .030\" (0.8 mm) and .035\" (0.9 mm)\u003c\/li\u003e\n \u003c\/ul\u003e\n \u003ch3\u003eWelder and Gas Requirements\u003c\/h3\u003e\n \u003cp\u003eUse a MIG setup that accepts a 4\" (102 mm), 2 lb (0.9 kg) spool and the selected wire diameter. Follow the applicable stainless-steel shielding-gas procedure.\u003c\/p\u003e","brand":"YesWelder","offers":[{"title":"1 PK \/ .030\"","offer_id":40362506256493,"sku":"ER308L-2LB-0-8","price":29.0,"currency_code":"USD","in_stock":true},{"title":"1 PK \/ .035\"","offer_id":45480416084077,"sku":"ER308L-2LB-0-9","price":29.0,"currency_code":"USD","in_stock":true},{"title":"3 PK \/ .030\"","offer_id":41843970965613,"sku":"ER308L-2LB-0.8 3PK","price":80.0,"currency_code":"USD","in_stock":true},{"title":"3 PK \/ .035\"","offer_id":45480416116845,"sku":"ER308L-2LB-0.9 3PK","price":80.0,"currency_code":"USD","in_stock":false},{"title":"5 PK \/ .030\"","offer_id":41843970998381,"sku":"ER308L-2LB-0.8 5PK","price":120.0,"currency_code":"USD","in_stock":true},{"title":"5 PK \/ .035\"","offer_id":45480416149613,"sku":"ER308L-2LB-0.9 5PK","price":120.0,"currency_code":"USD","in_stock":false}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0024\/3249\/9821\/files\/ER308030_StainlesssteelweldingwireER308035_Stainlesssteelweldingwire_43c55c2f-656c-4052-b4fd-58d62cf89438.jpg?v=1685601043","url":"https:\/\/pay.yeswelder.com\/products\/stainless-steel-mig-solid-wire-er308l","provider":"YesWelder","version":"1.0","type":"link"}