{"title":"Welding Gauge","description":"","products":[{"product_id":"welding-chipping-hammer-28oz-carbon-steel","title":"LTG01 28 oz Welding Chipping Hammer","description":"\u003cp\u003eLTG01 uses a one-piece forged carbon-steel body with pointed and chisel ends for post-weld slag and spatter removal. Its rubber grip helps reduce vibration and improve control.\u003c\/p\u003e\n \u003ch3\u003eFor Weld Cleanup\u003c\/h3\u003e\n \u003cp\u003eUse the pointed and chisel ends to break and lift slag or spatter after the weld has cooled to a safe handling condition. Wear eye and face protection because chips can travel when struck.\u003c\/p\u003e\n \u003ch3\u003eKey Specifications\u003c\/h3\u003e\n \u003cul\u003e\n  \u003cli\u003e\n\u003cstrong\u003eWeight:\u003c\/strong\u003e 28 oz\u003c\/li\u003e\n  \u003cli\u003e\n\u003cstrong\u003eMaterial:\u003c\/strong\u003e One-piece forged carbon steel\u003c\/li\u003e\n  \u003cli\u003e\n\u003cstrong\u003eGrip:\u003c\/strong\u003e Anti-slip, vibration-reducing rubber\u003c\/li\u003e\n \u003c\/ul\u003e\n \u003ch3\u003eUse Boundary\u003c\/h3\u003e\n \u003cp\u003eThis tool is designed for weld cleanup. Do not use it as an axe, sledgehammer or pry bar.\u003c\/p\u003e","brand":"YesWelder","offers":[{"title":"Default Title","offer_id":43587455352941,"sku":"LTG01","price":26.0,"currency_code":"USD","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0024\/3249\/9821\/files\/LTG01_5.jpg?v=1761501872"},{"product_id":"portable-welding-rod-oven-temperature-controlled-electrode-storage-oven","title":"BWX-01 Portable Temperature-Controlled Welding Rod Oven","description":"\u003cp\u003eBWX-01 provides adjustable heated storage for compatible covered electrodes in the shop or field. Its 110V input and 85°F to 300°F temperature range support holding requirements that vary by electrode classification and manufacturer.\u003c\/p\u003e\n\u003ch3\u003eHeated Electrode Storage\u003c\/h3\u003e\n\u003cp\u003eUse the oven to hold compatible covered electrodes under controlled heat and reduce moisture pickup during storage. Electrode storage and reconditioning requirements vary by classification and manufacturer, so follow the instructions supplied with the electrodes.\u003c\/p\u003e\n\u003ch3\u003eCapacity Comparison\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e15 lb (6.8 kg) model:\u003c\/strong\u003e Holds electrodes up to 14\" (356 mm)\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003e24 lb (10.9 kg) model:\u003c\/strong\u003e Holds electrodes up to 17\" (432 mm)\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003ch3\u003eKey Specifications\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003eInput:\u003c\/strong\u003e 110V AC\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003eTemperature range:\u003c\/strong\u003e 85-300°F (29-149°C)\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003eIncluded:\u003c\/strong\u003e Oven, power cord and user manual\u003c\/li\u003e\n\u003c\/ul\u003e","brand":"YesWelder","offers":[{"title":"15 lb","offer_id":45530414514285,"sku":"BWX-01","price":139.0,"currency_code":"USD","in_stock":true},{"title":"24 lb","offer_id":45530414547053,"sku":"BWX-02","price":169.0,"currency_code":"USD","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0024\/3249\/9821\/files\/PortableWeldingRodOven_2.jpg?v=1783328811"}],"url":"https:\/\/pay.yeswelder.com\/collections\/welding-gauge.oembed","provider":"YesWelder","version":"1.0","type":"link"}