E71T-GS is a self-shielded wire for all-position, single-pass welding on mild and carbon steel without external shielding gas. Choose the spool weight that fits the welder; FLUX-135PRO-A supports the 2 lb spool only.
Materials and Applications
- Mild steel and carbon steel
- Outdoor repair, fabrication, farm equipment, construction, and DIY work
Choose the Right Spool
2 lb spool: A compact choice for portable welding, occasional repairs, and machines with smaller spool compartments.
10 lb spool: An 8" spool that reduces spool changes during longer fabrication and repair work.
Works With
2 lb and 10 lb spools:
- YESWELDER DP200
- YESWELDER MCT520-A
- YESWELDER MIG-205DS-PRO
- YESWELDER MIG-250PRO-A
- YESWELDER MP200-PRO
- YESWELDER YWM-160
2 lb spool only:
- YESWELDER FLUX-135PRO-A
Key Specifications
- Classification: E71T-GS
- Process: Flux-Cored
- Shielding gas: Not required
- Spool weight options: 2 lb (0.9 kg) and 10 lb (4.5 kg)
- 10 lb (4.5 kg) spool diameter: 8" (200 mm)
- Wire diameter options: .030" (0.8 mm) and .035" (0.9 mm)
- Pack quantities: 1 PK, 3 PK, and 5 PK
- Welding use: All-position, single-pass welding